All grades

Reset criteria

6 grades

Select up to 3 grades to compare them
Show by:

Powder metallurgy HSS

Standards

  • Europe : PMHS 2-2-2
  • Germany : 1.3397

Delivered Hardness

  • Soft annealed : 220 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Conventional HSS

Standards

  • Europe : HS 6-5-2
  • Sweden : SS 2722
  • Japan : SKH51
  • Germany : 1.3343
  • USA : AISI M2

Delivered Hardness

  • Soft annealed : 250 HB
  • Cold drawn : 275 HB
  • Cold rolled : 275 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

Not standardized

Delivered Hardness

  • Soft annealed : 280 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : PMHS 4-3-8
  • Germany : 1.3352

Delivered Hardness

  • Soft annealed : 290 HB
  • Cold drawn : 305 HB
  • Cold rolled : 305 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : PMHS 6-5-3-8
  • Sweden : SS 2726
  • Germany : 1.3294

Delivered Hardness

  • Soft annealed : 290 HB
  • Cold drawn : 305 HB
  • Cold rolled : 305 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

Powder metallurgy HSS

Standards

  • Europe : PMHS 6-5-3C
  • Sweden : SS 2725
  • Japan : JIS SKH53
  • Germany : 1.3395
  • USA : AISI M3:2

Delivered Hardness

  • Soft annealed : 260 HB
  • Cold drawn : 285 HB
  • Cold rolled : 285 HB

Properties

Machinability

Wear Resistance

Toughness

Hot hardness

Grindability

Forms

You're consulting 6 over 6 grades

Select up to 3 grades to compare them